Dry rot is timber decay caused by the fungus Serpula lacrymans, which needs damp wood and can reach timber beyond the first wet spot.

What is dry rot?

Dry rot is the decay of timber by the fungus Serpula lacrymans. The Slovak term is drevomorka. The name misleads. The fungus needs wet wood to start. The Historic Scotland technical advice note says that neither wet rot nor dry rot attacks wood with a normal moisture content. It is called "dry" because the wood is often dry to the touch after the attack. The Monuments Board names roof leaks, wet backfill and damp rubble as common sources of the moisture.

How does dry rot differ from wet rot?

Historic Scotland names two differences. Dry rot fungi tend to decay wood at a lower moisture content than wet rot fungi, and they leave the wood in a dry state. The fungus can also move water to a limited extent from one place to another, so once it is established it persists and spreads. The table compares dry rot with the cellar fungus Coniophora puteana, one of the other building rots in the same note.

FeatureDry rot (Serpula lacrymans)Cellar fungus (Coniophora puteana)
Fruit bodyRusty redOlive green to brown, rarely seen
StrandsBrittle when dryBlack or brown
Wood after attackBrown, friable, often dry to the touchNot described in the note

The Slovak Monuments Board methodology gives one moisture rule for wood-decay fungi in general. They need at least 20 % wood moisture, with an optimum above 30 %, depending on the fungus. Telling the fungi apart on site is a specialist task.

What conditions does dry rot need?

Historic Scotland lists the conditions in one table. The Monuments Board and the conservation article by Carey and Grant agree on the 20 % line. Below about 20 % wood moisture the decay stops.

FactorCondition that favours dry rot (Historic Scotland)
Wood moisture contentAbove 20 %, timber is at risk
Air humidityRelative humidity above 90 %
Air movementStagnant air
TemperatureConstant, 4 to 24 °C. Above 24 °C kills the fungus
MasonryTimber that penetrates damp masonry

The same note says wood needs more than 20 % moisture for dry rot to grow from mycelium, and 30 % from spores. It calls these figures general and hard to measure. Seasoned wood sits at around 12 to 16 %. The Monuments Board adds that wood in roofed spaces usually has 10 to 16 % moisture. In spaces without ventilation it can reach a critical 18 to 20 %. A dry-looking room can therefore still hold wet timber.

Can dry rot spread through masonry?

The sources stress different points. Carey and Grant write that the strands can grow through and across masonry, but the fungus gets no nourishment from it. They add that the strands conduct water only to a limited degree, and good ventilation can negate this. Historic Scotland adds that the fungus needs metal ions from masonry as well as nutrients from wood. It grows thickly where wood meets masonry, for example behind lath and plaster. The Monuments Board says dry rot can cross dry areas and areas with no wood. Read together, the fungus is bound to wood for food, but it can bridge masonry to reach more wood.

A new outbreak can also start from spores. Kauserud and colleagues, in a 2012 review, found that indoor populations in Europe mainly spread through sexual spores, the basidiospores. Historic Scotland notes that a fruit body releases spores in very large numbers, so spores are always in the air. Stopping spores is not a workable plan. Controlling the moisture is.

What are the signs of dry rot?

Historic Scotland describes the final stage of attack as cuboidal cracking along and across the grain. The wood turns uniformly brown and friable, and is often dry to the touch. The fungus may show a rusty red fruit body, brittle strands and fluffy, cotton-wool mycelium. A flat grey mycelium means the outbreak is probably no longer growing, and a dark yellow or brown mycelium means it is dying or dead. The note admits that deciding whether an outbreak is alive is imprecise. It adds that the moisture stays a risk even when the fungus is dead.

Carey and Grant recommend regular visual inspection of the fabric for water entry and moisture readings of vulnerable timber with a hand-held probe. A survey that only looks at the surface can miss decay behind finishes.

How is dry rot repaired?

The sources agree on the order. First find the outbreak and its cause, which the Monuments Board lists as moisture, lack of light and lack of air movement. Then remove the cause of the moisture, then repair. They differ on scope.

StepMonuments Board methodologyHistoric Scotland
Infected timberRemove all infected wood. Separate the outbreak from the rest of the buildingFloor joists: cut back to the last visible signs of decay, then partner or splice. Many practitioners still cut back 1 m beyond
MasonryClean mechanically, flame and treat masonry grown through with mycelium and thick grey strandsDry the masonry by heating, ventilation and dehumidification. Drilling and injecting chemicals is not necessary, because it adds moisture
Infected puggingNot describedRemove it. The effectiveness of modern substitutes for sound insulation is questionable
New timberTreat it first, ventilate the space and keep it at about 15 % moistureSupport new joist ends and isolate them from walls with metal hangers or damp-proof material

Carey and Grant state that removing all affected timber is destructive but necessary in principle. They say plaster comes off only where timber is embedded in the walls and at risk. They also say local chemical treatment of masonry can form a barrier between the fungus and the wood. It is not a substitute for drying the building, and drying can take years. The Monuments Board says the designer and the eradication specialist set the scope together, and that a skipped step leads to a new outbreak. Only pressure impregnation or long steeping reliably protects new timber against dry rot. See timber preservative and beam-end repair.

Which parts of an old ceiling are at risk?

The Monuments Board names wet backfill and damp rubble as sources of dry rot, and says fresh concrete must not stay in contact with timber. It also gives a warning case. Tie beams covered with expanded clay backfill gave dry rot the conditions to spread. See ceiling backfill. A vapour barrier in a timber ceiling raises the risk. The methodology lists plastic film, plasterboard, fibre cement board, concrete, wood fibre board and particle board among the materials that can form one. Roof leaks, defective flashings, overflowing gutters and pipes in contact with timber are the usual water sources. Check the build-up before closing it with ceiling boarding. Wood-boring beetles can attack the same ceiling, but they need a different treatment. See wood-boring insects.

Is dry rot the same as damp?

No. Damp is the moisture in the building. Dry rot is a fungus that has taken hold of the timber because of that moisture. Damp is the cause to remove, and dry rot is one result of it.

Frequently asked questions

Is dry rot the same as wet rot?
No. Historic Scotland says dry rot fungi decay wood at a lower moisture content than wet rot fungi and leave the wood dry. The fungus can also move water to a limited extent, so it persists and spreads. Both need damp wood to start.
At what moisture content does dry rot grow?
Historic Scotland gives wood moisture above 20 % as the level at which timber is at risk. Carey and Grant say decay stops below about 20 %. The Slovak Monuments Board says drying below 20 % stops fungi but not insects.
Can dry rot spread through brick or stone?
The strands can grow through and across masonry, but the fungus gets no food from it, say Carey and Grant. Historic Scotland adds that it takes metal ions from masonry. The Monuments Board says it can cross dry areas and areas with no wood.
Is removing the visibly rotten timber enough?
No. The cause of the moisture must be removed. The Monuments Board requires removal of all infected wood and finding the outbreak. Historic Scotland cuts joists back to the last visible signs of decay, and many practitioners cut 1 m further.
Is drilling and injecting the wall a standard cure?
Sources differ. Historic Scotland calls drilling and chemical injection of infected masonry unnecessary because it adds moisture. The Monuments Board has masonry cleaned, flamed and treated. Carey and Grant call chemical treatment of masonry a barrier, not a substitute for drying.
How does a new outbreak start?
Kauserud and colleagues found that indoor populations spread mainly through basidiospores. Spores are always in the air, so the control is to keep wood below the moisture level the fungus needs.

Sources

  1. Dry Rot and its Treatment in Historic Buildings · Janice Carey and Colin Grant, reproduced from The Building Conservation Directory (1999), buildingconservation.com · Whole article
  2. Evolutionary origin, worldwide dispersal, and population genetics of the dry rot fungus Serpula lacrymans · Kauserud H., Knudsen H., Högberg N., Skrede I. Fungal Biology Reviews 26(2), 84-93, 2012, DOI 10.1016/j.fbr.2012.08.001; record via FAO AGRIS · Abstract
  3. Technical Advice Note 24: The Environmental Control of Dry Rot · Historic Scotland (now Historic Environment Scotland), 2002 · 2.2 Wet and dry rot; 2.3.2 to 2.3.4; Table 2 and Table 3; Illustration 5; 6.3.2.2 Floor joists; 6.3.2.8 Pugging; 6.3.2.11 Masonry
  4. Metodika princípov rozhodovania Pamiatkového úradu SR, časť 11, Statika, technické normy a sanácie, Príloha č. 3: Ochrana dřeva · Pamiatkový úrad Slovenskej republiky (author Jan Vinař) · 1 Ochrana dreva proti vlhkosti; 2.4; 2.5; 2.6 Likvidácia napadenia dreva
  5. Metodika princípov rozhodovania Pamiatkového úradu SR, časť 9, Drevo a drevené stavby, Príloha č. 2: Typy poškodení dreva · Pamiatkový úrad Slovenskej republiky (authors Jaroslav Hrivnák, Michal Kloiber) · 2 Biotické poškodenie dreva (table)
  6. Metodika princípov rozhodovania Pamiatkového úradu SR, časť 11, Statika, technické normy a sanácie, Príloha č. 8: Historická stavba a její nosné konstrukce · Pamiatkový úrad Slovenskej republiky (author Jan Vinař) · 9.1 Pôsobenie vonkajších činiteľov
  7. Metodika princípov rozhodovania Pamiatkového úradu SR, časť 11, Statika, technické normy a sanácie, Príloha č. 6: Dřevěné konstrukce · Pamiatkový úrad Slovenskej republiky (author Jan Vinař) · 3.4 Posuzování a oprava stropů; 3.5 Tepelné, zvukové a protipožární izolace stropů