Ceiling backfill

Ceiling backfill is the loose layer, often old rubble or slag, laid on the boarding of a timber beam ceiling under the floor.

Ceiling backfill is the loose layer that lies on the boarding of an old timber beam ceiling, between the beams and the floor above.

The Slovak term is zásyp stropu or násyp. The Monuments Board of Slovakia (Pamiatkový úrad SR) says that in vaults and timber beam ceilings the fill had the insulating function. It was usually building rubble. The methodology is written for monuments, so for an ordinary house it is technical guidance, not a legal rule. See ceiling boarding for the layer under the fill and floor joists for the beams.

What did the backfill do?

The fill worked with the air gap between the ceiling structure and the plastered soffit. The ceiling methodology says that the air gap together with the fill raises the thermal insulation, the fire parameters and the acoustic properties of the ceiling. In 19th-century ceilings with a plastered soffit, the boarding sat on laths fixed to the sides of the beams. The layer of fill above the top of the beams then gave impact sound insulation. The sources give no figures for these effects.

The fill also loads the ceiling. The methodology gives building rubble a weight of about 1300 kg/m³. A layer 10 cm thick therefore adds about 130 kg per m² (0.1 m × 1300 kg/m³). The engineer must count this load when the fill is removed, kept or replaced.

What is the backfill made of?

Traditional fill was mostly building rubble, that is knocked-off plaster, fragments of demolished structures and soil. Many fills contain a large share of organic admixtures such as chaff, wood shavings, sawdust and straw. From the 19th century slag (škvára) was also used. In attics, clay screeds and clay and straw layers (lepenica) added to the insulation of the fill. The table lists what the methodology says about each material.

MaterialWhat the methodology says
Building rubbleAbout 1300 kg/m³. Often contains organic admixtures. Rubble from the site may be used again if it holds no organic admixtures and was stored dry
Slag (škvára)Used from the 19th century. It must not contain unburnt coal or certain elements, above all sulphur. A test certificate (atest) must confirm that it is suitable
Recycled rubbleWithout risk if it is certified for use in a building
Expanded clay, perlite, foam glassIn common use since the second half of the 20th century. Light, not absorbent, high thermal resistance. Low weight can help in ceilings but may not suit vaults

What goes wrong when backfill gets wet?

Wet fill is a moisture source for the timber around it. The timber protection annex says that fills and clay screeds soaked during construction, and damp rubble stored or brought on site, are often a source of moisture and of dry rot. The ceiling methodology adds that organic admixtures become a source of mould and fungi when the fill is soaked. In neglected buildings, clay attic screeds are an indirect source of fungal attack on timber ceilings. The annex also lists soaked fills among the results of roof leaks. Repair the roof and other water sources before work on the fill, and keep reusable rubble dry.

Is it a mistake to remove the backfill?

Often, yes. The ceiling methodology names the removal of the clay upper fill of a ceiling, for example for hygiene reasons, as a frequent mistake. It can move the dew point, change the moisture conditions and start the deformation of the load-bearing timber. For a historically valuable ceiling the consequences for the plastered soffit can be severe. The methodology asks that any major change of the build-up, for example to improve thermal insulation, is checked by thermal and static diagnostics.

For monuments the Monuments Board goes further. It says that fills are part of the heritage value and often hold evidence of how the building developed. They can hold remains of old roofing, stove tiles, fittings, tools, sherds, documents and old prints. These fills should not be cleared. If clearing is necessary, objects of historic or informational value should be sorted out. Old layered fills of vaults should be cleared under the supervision of an authorised archaeological organisation.

Can modern materials replace the original backfill?

The methodology says that similar loose materials are suitable as replacement and that their properties must always be checked. It also says that returning the original fill to a ceiling attacked by fungus is a problem. Heating the fill to a temperature that kills the pests is named as a possibility that must always be checked in detail. Fills and thermal insulation in historic buildings should be breathable. The timber protection rules always apply. The methodology gives a warning example: tie beams covered with expanded clay, which created the conditions for dry rot to spread.

Historic Scotland, a foreign source, says that infected pugging and deafening should be removed, above all around the edge of rooms. It says that modern substitutes can restore acoustic insulation between floors, but that their effectiveness compared with traditional materials is questionable. Check the acoustics of the new build-up.

What should you check before work on the backfill?

The methodology requires a detailed survey before any intervention in a ceiling of a protected building. The survey finds the real form of all elements, their function, bearing, joints and condition. In phases, probes during design show the build-up and an area survey during construction fixes the scope. The list below is a practical reading of the sources for any old ceiling.

CheckWhySource
Layers and objects in the fillOld fills can be layered and can hold objects of historic valueAnnex 6, section 3.5
Organic contentChaff, shavings and straw feed mould and fungi when wetAnnex 6, section 3.5
Moisture sourceWet fill and damp rubble are named dry rot sourcesAnnex 3, section 1
Rot in boarding and beamsInfected pugging should be removedTAN 24, section 6.3.2.8
Slag or recycled rubbleSuitability needs a test certificate or certificationAnnex 6, section 3.5
Dew point and structureRemoving fill can change bothCeilings methodology, section 3.1

Check the beam ends for dry rot before any decision. The timber preservative rules of the annex still apply where the fill stays.

Frequently asked questions

Why keep the old backfill instead of clearing it out?
The Monuments Board methodology says that the fill had the insulating function and that the layer above the beams gave impact sound insulation in 19th-century ceilings. It calls the fills part of the heritage value of a monument. Removing the clay upper fill can also move the dew point and start deformation of the timber.
Is building rubble safe to put back?
Only if it holds no organic admixtures and was stored dry. The methodology says that recycled rubble is without risk when it is certified for use in a building. Wet or organic fill leads to mould, fungi and dry rot.
Can slag be reused in a timber ceiling?
Slag was used as fill from the 19th century. It must not contain unburnt coal or certain elements, above all sulphur. A test certificate must confirm that it is suitable.
Are expanded clay, perlite or foam glass good replacements?
The methodology calls them light, not absorbent and high in thermal resistance. Low weight can help in ceilings. It warns that expanded clay laid over tie beams created the conditions for dry rot, so timber protection rules still apply.
What does 10 cm of rubble backfill weigh?
About 130 kg per m². The methodology gives building rubble a weight of about 1300 kg/m³, and 0.1 m × 1300 kg/m³ is 130 kg/m². The engineer checks the load before the fill is changed.
What should be checked before work on the fill?
Check the layers and objects in the fill, its organic content, the moisture source, rot in the boarding and beams, and the dew point. In a protected building a detailed survey must come first.

Sources

  1. Metodika princípov rozhodovania Pamiatkového úradu SR, časť 11, Statika, technické normy a sanácie, Príloha č. 6: Dřevěné konstrukce (Czech text) · Pamiatkový úrad Slovenskej republiky (author Jan Vinař) · 3.3 Průzkum stropů; 3.5 Tepelné, zvukové a protipožární izolace stropů
  2. Metodika princípov rozhodovania Pamiatkového úradu SR, časť 11, Statika, technické normy a sanácie, Príloha č. 3: Ochrana dřeva (Czech text) · Pamiatkový úrad Slovenskej republiky (author Jan Vinař) · 1 Ochrana dřeva proti vlhkosti; ochrana při realizaci stavby
  3. Metodika princípov rozhodovania Pamiatkového úradu SR, časť 8, Stavebná časť, stavebné prvky: Podlahy, stropy, schodiská, časť Stropy · Pamiatkový úrad Slovenskej republiky (Plán obnovy a odolnosti SR, Komponent 2) · 3.1 Dřevěné stropy
  4. Technical Advice Note 24: The Environmental Control of Dry Rot · Historic Scotland, Technical Conservation, Research and Education Division · 6.3.2.8 Pugging/deafening