Crystalline waterproofing

Crystalline waterproofing is a cement-based admixture or coating that reduces water penetration into concrete and helps fine cracks heal.

Crystalline waterproofing is a cement-based admixture or coating that reduces water penetration into concrete and helps fine cracks heal. In Slovak it is called kryštalická hydroizolácia. It acts inside the concrete and does not form a separate layer, so it differs from a pre-applied membrane and from bentonite waterproofing.

What is crystalline waterproofing?

It is a group of cement-based products in two forms. An integral admixture is added to the concrete mix. A surface slurry is applied to hardened concrete. One maker, Schomburg, calls its admixtures BETOCRETE products for integral sealing of concrete, and its slurry AQUAFIN-IC a cement-bound, capillary-active sealing slurry for concrete substrates.

A peer-reviewed study in the journal Materials (Gojević, Ducman and Netinger Grubeša, 2021) places such admixtures in an ACI 212.3R-16 class. The class is permeability-reducing admixtures for hydrostatic conditions. The study describes them as products for watertight structures such as tanks and foundations.

How does crystalline waterproofing work?

Makers describe the effect as crystal growth in the pores. BauNetz Wissen, a site sponsored by the German concrete industry, describes one product that forms needle-shaped crystals from moisture and cement components. It reports that growth needs water and temperatures above 5 °C. Growth stops when a capillary pore dries out and starts again when water returns. The article words its growth depths as claims of the maker, so this page does not repeat them.

The research is more cautious about the cause. The 2021 study explains the reduced water penetration and the healed cracks by several mechanisms. They include calcium silicate hydrate gel from unreacted clinker grains, carbonates, and a gel from magnesium-based additives. The study also found that the standard 28-day curing of the permeability test may be too short for the full effect to develop.

How much crack can crystalline waterproofing seal?

Only fine cracks. The 2021 study lists healed crack widths from earlier work. Some studies report complete healing up to 0.1 mm, one up to 0.3 mm and two up to 0.4 mm. In its own tests, more cracks of 0.15 mm healed in mixes with the admixture than in the reference mixes. Some cracks up to 0.15 mm still did not heal completely.

The makers state higher values for their own products, as the table shows. These are the maker's values under its own test conditions. They are not values for every crystalline product.

FormExample productUseValue stated by Schomburg
Powder admixtureBETOCRETE-CP360-WPAdded to the concrete mixCrack healing up to 0.5 mm, dosage 0.75 to 1.25 per cent of the cement content
Liquid admixtureBETOCRETE-CL210-WPAdded to the concrete mixCrack healing up to 0.5 mm, dosage 1.75 to 2.25 per cent of the cement content
Surface slurryAQUAFIN-ICApplied to concrete, stated to work also against negative water pressureConsumption about 0.75 to 1.5 kg/m2
Crystalline joint sheetAQUAFIN-CJ5Placed in construction jointsCracks up to 0.4 mm can close on contact with water

The table values come from the 2019/20 product programme and the 2026 planning guide of that maker. Check them against the current data sheet before use.

Where is crystalline waterproofing used?

The programme lists AQUAFIN-IC for outside and inside sealing of basements, lift shafts, foundations, piled foundations and ground slabs. It also lists it for drinking-water and process-water tanks, retention basins and water treatment plants, and under screeds. The maker states that the slurry is tested to DVGW W 270 and W 347 for drinking-water tanks. The admixtures are stated as certified to EN 934-2.

Is it part of DIN 18533?

DIN 18533-1 is the German standard for sealing of components in contact with soil. DIN Media lists the 2026-06 edition as current. Its scope excludes watertight (WU) structures, and the crystalline admixtures are meant for such concrete. The standard grades crack movement in the substrate, which the free table of contents lists under crack classes.

Crack classCrack width changeCrack-bridging class
R1-EUp to 0.2 mmRÜ1-E, low
R2-EUp to 0.5 mmRÜ2-E, moderate
R3-EUp to 1.0 mm, offset up to 0.5 mmRÜ3-E, high

This table is reproduced in the Schomburg planning guide of 15 July 2026, not read from the standard. In the guide's table, flexible mineral sealing slurries are named for the classes R2-E and R3-E. It does not list crystalline products in those rows, so do not assume a crystalline product bridges the larger crack classes.

Is crystalline waterproofing a substitute for a watertight structure?

No source read for this page presents it as a substitute. BauNetz Wissen describes a crystalline product as an admixture used to make watertight concrete, and also for repairing existing surfaces and cracks. The 2021 study found that the effect depends on the mix and on the curing time. Even with the admixture, not every crack of 0.15 mm healed. A crack that is wide, dry or still moving falls outside what these sources describe.

See watertight concrete structure for the design of the concrete itself, and liquid-applied waterproofing for a coating that bridges cracks.

What should an architect check before specifying it?

  • The crack width the maker states, and the test conditions behind it.
  • The dosage as a share of the cement content for an admixture, or the consumption per square metre for a slurry.
  • The certificates the maker lists for the intended use. Examples are EN 934-2 for an admixture and DVGW W 270 and W 347 for a drinking-water tank.
  • Whether the substrate and the curing allow the product to work. The 2021 study showed that curing time and mix change the result.

Frequently asked questions

What is crystalline waterproofing?
It is a group of cement-based products that reduce water penetration into concrete. They are either added to the concrete mix as an admixture or applied to hardened concrete as a slurry. In Slovak the term is kryštalická hydroizolácia.
Does crystalline waterproofing seal cracks?
Only fine ones. A 2021 study in Materials lists healed crack widths of 0.1 to 0.4 mm in earlier work. The maker Schomburg states healing up to 0.5 mm for its admixtures and up to 0.4 mm for its joint sheet. Wider or moving cracks fall outside these values.
Is crystalline waterproofing enough on its own for a basement?
No source read for this page presents it as a substitute for a designed watertight structure. BauNetz Wissen describes it as an admixture used to make watertight concrete or to repair concrete.
Can a crystalline slurry be used inside a basement?
The maker lists AQUAFIN-IC for outside and inside sealing of basements and says it works also against negative water pressure. Check the current data sheet for the substrate and the pressure.
How is crystalline waterproofing different from bentonite?
A crystalline product is cement-based and acts in the concrete pores. Bentonite is a clay sheet that swells and needs contact pressure, according to BauNetz Wissen and the maker CETCO.

Sources

  1. The Effect of Crystalline Waterproofing Admixtures on the Self-Healing and Permeability of Concrete · Materials 14(8), 1860 (MDPI), Gojević, Ducman, Netinger Grubeša, peer-reviewed · Introduction, Section 4 Conclusions
  2. Betonabdichtung durch Kristallbildung · BauNetz Wissen, Beton section, sponsored by the Deutsche Zement- und Betonindustrie (InformationsZentrum Beton) · Whole article (about the product Xypex)
  3. DIN 18533-1:2026-06 Abdichtung von erdberührten Bauteilen, Teil 1: Anforderungen, Planungs- und Ausführungsgrundsätze (Waterproofing of elements in contact with soil, Part 1) · DIN Media (Beuth) · Catalogue page: Ausgabedatum, Anwendungsbereich
  4. DIN 18533-1:2026-06 table of contents (Inhaltsverzeichnis) · DIN (NA Bau, free table of contents download) · 5.5.2 Rissklassen
  5. Produktprogramm 2019/20: Abdichtungssystem Betonbau · Schomburg (manufacturer product programme) · pp. 4 to 6: BETOCRETE-CP360-WP, BETOCRETE-CL210-WP, AQUAFIN-IC, ASOCRET-IM
  6. Planungs- und Anwendungsratgeber für die Bauwerksabdichtung und Instandsetzung · Schomburg (manufacturer planning and application guide, version dated 2026-07-15) · p. 24 (crystalline joint sheet AQUAFIN-CJ5); p. 30 (DIN 18533 criteria, crack classes and crack-bridging classes, citing DIN 18533-1; DIN 18533 title)