Shrinkage crack

A shrinkage crack is a crack that forms when a material loses water and contracts while something holds it in place.

What is a shrinkage crack?

A shrinkage crack is a crack that forms when a material loses water and gets smaller while something holds it in place. The NIST report on curing high-performance concrete speaks of internal stresses that arise when shrinkage meets restraint. It says creep relieves these stresses and so reduces shrinkage cracking. The edges of the crack pull apart as the layer contracts.

The Pamiatkový úrad SR guidance for historic buildings lists the shrinkage cracks that come from volume changes of some materials. It also names the drying of timber, the creep of masonry and the consolidation of the ground. It says you must tell these cracks apart from static cracks, which come from loads. You must also tell them apart from dilatation cracks, which come from dynamic and temperature loads. A shrinkage crack is a different problem from a crack that comes from overload or from moving ground. Structural crack covers that problem. The name describes the mechanism, not the severity. The guidance warns that different causes can give defects that look alike, so check the crack before you decide.

Where do shrinkage cracks come from?

Two sources read for this article describe the mechanism. The NIST report covers concrete. The Pamiatkový úrad guidance covers cement mortar. Table 1 summarises both.

SettingWhat the source saysSource
Fresh concrete surface, between finishing and final setCracks form when evaporation exceeds the rate at which water reaches the surfaceNIST, section 5.9
Silica-fume concrete with little bleedingMore prone to plastic shrinkage cracking than ordinary concreteNIST, section 5.9
Cement mortar as it hardensThe mortar shrinks and cracks form in itPamiatkový úrad SR, section 9.3

No source read for this article describes the mechanism for plaster or render. Ask the applicator which mix they used and how they protected the surface while it cured. Ask also whether the crack appeared in the first days or weeks. Those answers help the engineer judge the cause.

The Pamiatkový úrad guidance says narrow cracks in cement mortar let moist air in, and water can then run into the masonry. Capillary action stops the moisture leaving through such a narrow crack. The guidance says this shows most in the joints of wall tops, parapets, cornices and exterior paving. It adds that filling cracks by pointing or injection makes the masonry more uniform and keeps moisture out.

How is a shrinkage crack different from a structural crack?

The British Building Research Establishment (BRE) sorts cracks into six categories, from 0 to 5. The categories link the width and number of cracks to the type of repair. BRE built the scheme from a study of 130 properties that suffered subsidence. The scheme is a rough guide to how serious a crack is, and BRE does not present it as a classification of shrinkage. A reader who uses it for a shrinkage crack should keep that limit in mind.

BRE categoryWhat BRE saysWhat it affects
0, 1 and 2Aesthetic, with crack widths up to 5 mmAppearance, and BRE says only redecoration is needed
3 and 4ServiceabilityWeather-tightness, and how doors and windows operate
5StabilityLikely to need structural intervention

BRE itself calls the scheme a simplification. It also says that widening over time can change the category. Width alone therefore does not separate a shrinkage crack from a structural one. The cause and the behaviour over time do.

How do you check a crack before deciding what to do?

The Building Conservation Directory, in an article by the engineer Clive Richardson, gives a few practical checks. They help to judge whether the crack is old or still moving. The Pamiatkový úrad guidance gives the wider rule: clarify the cause of every defect.

CheckWhat it tells youSource
Crack faces: fresh and clean edges, or old paint and filler insideRichardson says careful examination can show the direction of movement and whether it continuesRichardson
Width measured again after a periodWhether the crack is growing. BRE links the category to thisBRE
Cause unclear, or movement possibly progressiveMonitoring is warranted. A crack gauge records changeRichardson
Direction of the crackCrack directions show the directions of the forcesPamiatkový úrad SR, section 4

Richardson writes that you should examine cracks to find their cause and not fill them rigidly. A rigid fill may restrict cyclical movement and let the problem escalate. Where damage is significant, BRE advises calling a building professional. For movement that may come from the ground, see differential settlement.

When you write up an inspection, describe the crack in plain terms. Note its direction and its approximate width at both ends. Note whether it shows on one side or both sides of the wall. Note whether it is near a window or a door. This gives the engineer something to work from.

Can shrinkage cracks be prevented in new work?

The NIST report states the aim for silica-fume concrete: the surface must not dry at any time before the final curing measures begin. It quotes the ACI 234 guide on this. The guide recommends curing compound straight after finishing. It also recommends covering with wet burlap and plastic sheeting for at least 3 days, preferably 5 to 7 days. Until the covering goes on, it recommends fog misting or an evaporation retarder. Controlling the drying of the surface is the subject of concrete curing, which covers the timing and methods in more detail.

Richardson notes that walls in hard cement mortar, unlike older walls in lime mortar, need movement joints at frequent intervals. A planned control joint serves this purpose in new work. The sources read here do not give joint spacing, so ask the designer. Record the crack width, its position and the date of each reading. That record gives a baseline. Without it, you cannot tell later whether the crack grew.

Frequently asked questions

Is a shrinkage crack the same as a structural crack?
No. A shrinkage crack comes from a material changing volume, as when cement mortar shrinks while it hardens. A structural crack points to a defect in the structure. The Pamiatkový úrad SR guidance for historic buildings says you must tell the two apart, because different causes can give cracks that look alike. BRE sorts damage by width and effect, and its category 5 covers stability.
How wide can a shrinkage crack be before it matters?
The sources read for this article give no single width for shrinkage cracks. BRE's aesthetic categories run up to 5 mm, but they come from subsidence damage, and BRE calls its scheme a simplification. A wider crack that is stable can still be less serious than a narrow one that keeps growing.
Should I fill a shrinkage crack?
Find the cause first. Richardson writes that you should examine cracks to determine the cause and not fill them rigidly. The Pamiatkový úrad guidance adds that filling cracks in historic masonry, by pointing or injection, helps keep moisture out and makes the masonry more uniform. The cause decides the repair.
Why do cracks appear on a new concrete surface?
The NIST report describes plastic shrinkage cracks. They form on the exposed surface of newly placed concrete when water evaporates faster than bleed water reaches the surface. They can appear between the end of finishing and final set. Silica-fume concrete bleeds little, so it cracks more easily. The report says the surface must not dry out.
Why does cement mortar crack as it hardens?
The Pamiatkový úrad guidance says cement mortar shrinks as it hardens, and cracks form in it. Moist air and water can then enter the masonry through narrow cracks. The guidance names exterior joints in wall tops, parapets, cornices and paving as the places where this shows most.
When should a crack be monitored?
Richardson says to monitor when the cause is unclear or the movement may be progressing. A crack gauge that records the width over time shows whether the crack is changing. BRE also says that a changing width can change the category of a crack.

Sources

  1. Assessing cracks in houses · BRE (Building Research Establishment) · Crack categories 0 to 5; when to consult a professional
  2. Movement (structural movement in buildings) · The Building Conservation Directory, Clive Richardson · Dimensional instability; Assessment and conclusion
  3. Curing of High-Performance Concrete: Report of the State-of-the-Art (NISTIR 6295) · National Institute of Standards and Technology (Meeks and Carino) · 5.9 Early-Age Curing of Silica-Fume Concrete; discussion of shrinkage restraint and creep
  4. Príloha č. 8. Historická stavba a její nosné konstrukce (Statika, technické normy a sanácie) · Pamiatkový úrad SR (methodology by Jan Vinař) · 4. Statika stavby (úvod); 9.3 Ochrana před vlhkostí